Hi Kinetic,
What type of fillers are you using? and what type of mould did you use? It is very unusual for Fast Cast Polyurethanes to not go off unless something has gone very very wrong.
Was the resin measured out by weight? Also was Part A shaken so redistribute any settled sediment?
We have not heard of any problems with our Fast Cast resin, in fact I made a couple of small casts last night with no issues, so I am keen to try and work out what has gone wrong. So any information you can give would be useful to resolve the problem.
Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant
|