Sparky2305
Sparky2305
posted 10 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 10,
Visits: 69
Hi
Has anyone used the new Xencast P6 resin yet? I'm struggling with it as I type I have a part that has been curing for over an hour at 20 degrees plus as the mold was warm and the part is still green. I have mixed the same amount of fillers and pigment as I used to with the old system but the results with xencast seem terrible in comparison.
Like to hear anyone's experiences with it.
Thanks
Reply
Like
21
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
New Xencast fast cast resin
Sparky2305
-
10 Years Ago
Hi Kinetic, What type of fillers are you using? and what type of mould did you use? It is very...
Warren (Staff)
-
10 Years Ago
Hi Warren Silicone mold, a luminium trihydroxide filler, weight, well shaken and de-gassed. The...
Sparky2305
-
10 Years Ago
Hi Kinetic, Just picking up on this thread, had this issue been resolved. The Xencast P6 is our...
Matt (Staff)
-
10 Years Ago
Post Reply
Like
21
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search