Yes, even "pro-finish" is not completely "fixed" in the weave, it would be very difficult to use over any sort of curved surface if it was completely "locked" (It can be tricky over compound curves as it is)
"normal" 2/2 twill CF .. (The "bread'n butter stuff" ) is very loose, conforms ( & distorts) very easily..
I have on occasion "reinforced" the Pro-finish by spraying it with Cytec Aerofix 3 on the "misty" side .. when I wanted to absolutely sure that the edges did not fray (when making visible "cut-lines")
"Sapere Aude"... Dare to KNOW!
The written word is the only truly efficient vehicle for transmitting a complex concept from mind to mind...
103% of all people do not understand statistics...