By Ronny - 6/30/2015 10:50:33 PM
Hi, ive just recieved a roll of pro finish carbon from EC. Beeing new to this im supprised how "loose" the carbon was, and this was the pro finish. I expected to see some traces of resin as mentioned in the description of the product, but it looks to me like it is pure carbon fibre. Can anyone have a look at the pictures and tell if i got the right product?
Im not looking for a refund or anything, just curious if this in fact is the pro finish fabric.
Also there was some pollution on the fabric, if thats the right word, small pieces of paper/carton between the layers. Do you guys go over the fabric with a brush or anything before applying the resin?
|
By matthieutje65 - 7/3/2015 7:59:09 PM
reading your description it sounds like profinish
|
|