Group: Administrators
Posts: 214,
Visits: 782
|
Fill them with some resin. Will be tedious but necessary if you want to be able to just simply spray over.
You could try wiping resin on then off again so you only use a thin layer to fill the pinholes. Or just paint on another few thin layers of resin like you would do with carbon skinning.
You would of course need to sand it smooth again afterwards.
|