Hi,
So I've finished my Fieldhockey keeper Helmet...
No clearcoat was used.
I've used resin infusion but had some trouble with the vac bag and had a tiny little hole in it. it lost some vacuum after 8h I think...
Ive used the IN2 epoxy SLOW hardener...



So I would like to get a finnishing coat on it, what doe you think the best way is?
-Spraygunning clear epoxy on it
-Brush epoxy on it and let the excess epoxy drip of the part
-Spraygunning a topcoat (should have to buy it...so prefere the first option