Group: Forum Members
Posts: 2,
Visits: 3
|
Hi
I am currently making some bespoke motorcycle panels which are going to require a split mould. Given the flat-ish nature of the parts it would be easier to use your epoxy putty. Can I apply the same techniques shown in your split mould video just substituting the gel coat etc for putty?
I have also made my first split mould which was stressful but quite rewarding! It has a couple of small chips around the join lines where I wasn't thorough enough with either the release agent or the wax. Is there any way I can fill/repair these or is it best to just dress the part after manufacture?
|