Hi

I am currently making some bespoke motorcycle panels which are going to require a split mould. Given the flat-ish nature of the parts it would be easier to use your epoxy putty. Can I apply the same techniques shown in your split mould video just substituting the gel coat etc for putty?

I have also made my first split mould which was stressful but quite rewarding! It has a couple of small chips around the join lines where I wasn't thorough enough with either the release agent or the wax. Is there any way I can fill/repair these or is it best to just dress the part after manufacture?
By apelikemanthing - 11/11/2014 4:30:08 AM

Excellent thanks, that's going to make life a lot easier and, if it smells better, I may be able to avoid divorce for a little while longer....