Hi

I am currently making some bespoke motorcycle panels which are going to require a split mould. Given the flat-ish nature of the parts it would be easier to use your epoxy putty. Can I apply the same techniques shown in your split mould video just substituting the gel coat etc for putty?

I have also made my first split mould which was stressful but quite rewarding! It has a couple of small chips around the join lines where I wasn't thorough enough with either the release agent or the wax. Is there any way I can fill/repair these or is it best to just dress the part after manufacture?
Dravis
Dravis
Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)
Group: Forum Members
Posts: 592, Visits: 1.9K
Yes, You can, I find the epoxy putty to be excellent for smaller parts, and I have made several split moulds with it ..

I reality it just replaces both the coupling layer and the rest of the glassfibre layers in the process..

And you can work in a smaller workshop, and not have the smell to bother you...

You will have to use an Epoxy tooling gelcoat with it.  

So far I'm on the third bucket of 5 kg's of putty ... The moulds made from it are very strong, and will last for a lot of pulls from it, and are easily repaired.

"Sapere Aude"... Dare to KNOW!

The written word is the only truly efficient vehicle for transmitting a complex concept from mind to mind...

103% of all people do not understand statistics...

Do not adjust our mind, theres a fault in reality :-)
apelikemanthing
apelikemanthing
Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)
Group: Forum Members
Posts: 2, Visits: 3
Excellent thanks, that's going to make life a lot easier and, if it smells better, I may be able to avoid divorce for a little while longer....
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search