	Group: Forum Members 	        
    Posts: 1, 
    Visits: 20 
    
 
          
		     | 
				                       
                 
                
                    
			            I am going to vacuum bag a Carbon Fiber bar stool, using IN2 Resin, Soric and Carbon Fiber Tape at the edges of the Soric, like in the How To...Bonnet/Hood video. The stool will be like a 16-inch wide ribbon with a profile that looks like a "Z", and a Soric core. The total length is approximately 65-inches. I am in the US, and I cannot find Infusion Grade Spray Tack anywhere.
  What method/s (other than Spray Tack) could I use to hold the Carbon Fiber Tape, Cloth, and Soric in place?