I (probably like most) have tried various things when I don't have the right gear. I thought it might be good (if we can stand the humiliation) to post em up so everyone can see what works and what doesn't. I'll start.
I've tried covering a plug in vinyl to give a good surface as I was too lazy to seal it and paint it properly. I tried airelease vinyl that had several coats of wax on it and I got away with it. Yay! I tried a cheaper vinyl and it wrinkles like mad. I tried the airelease with fewer wax coats and got a slight bubbling. Worked once but probably not something I'll chance again.
I used 'antique pine' wax once when I'd run out of proper mould release.
|