Hello FLD,

Professional is as Professional does, no pikey practice here haha!
                .                                Kind Regards
                                          The Fibreglass King
FLD
FLD
Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)
Group: Forum Members
Posts: 468, Visits: 2.7K
I (probably like most) have tried various things when I don't have the right gear.  I thought it might be good (if we can stand the humiliation) to post em up so everyone can see what works and what doesn't.  I'll start.

I've tried covering a plug in vinyl to give a good surface as I was too lazy to seal it and paint it properly.  I tried airelease vinyl that had several coats of wax on it and I got away with it.  Yay!  I tried a cheaper vinyl and it wrinkles like mad.  I tried the airelease with fewer wax coats and got a slight bubbling.  Worked once but probably not something I'll chance again.

I used 'antique pine' wax once when I'd run out of proper mould release.