I (probably like most) have tried various things when I don't have the right gear.  I thought it might be good (if we can stand the humiliation) to post em up so everyone can see what works and what doesn't.  I'll start.

I've tried covering a plug in vinyl to give a good surface as I was too lazy to seal it and paint it properly.  I tried airelease vinyl that had several coats of wax on it and I got away with it.  Yay!  I tried a cheaper vinyl and it wrinkles like mad.  I tried the airelease with fewer wax coats and got a slight bubbling.  Worked once but probably not something I'll chance again.

I used 'antique pine' wax once when I'd run out of proper mould release.
Reply
FLD
FLD
Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)
Group: Forum Members
Posts: 468, Visits: 2.7K
ajb100 (04/05/2014)
I once used car body polish and wax as release agent for a bonnet I was doing, and it actually worked really well!


I'm rather suspiscious that car waxes and mould waxes are rather similar in composition.  I have wondered how my paint would fare with a coat of easylease.  Might also help get brake dust off the wheels!
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search