Being the cheat bastard that I am, I always reuse my (envelop) bag. Sealent tape on one end, reuseable snap lock on the other. Before I seal the bag, I drape a piece of the cheapy, 1mil plastic from Home Depot over bleeder and nothing sticks to the bag. Usually get 6-8 pieces from one bag.