carbon bonnet finishing


Author
Message
Matthieu Libeert
Matthieu Libeert
Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
sand the edge or entire part as well (if needed) then clearcoat everything and it should be fine

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




kidpaint
kidpaint
Supreme Being (778 reputation)Supreme Being (778 reputation)Supreme Being (778 reputation)Supreme Being (778 reputation)Supreme Being (778 reputation)Supreme Being (778 reputation)Supreme Being (778 reputation)Supreme Being (778 reputation)Supreme Being (778 reputation)
Group: Forum Members
Posts: 99, Visits: 676
Once sanded, do you re-epoxy the edge to see it, or the whole bonnet? I thought about sanding the edge then spraying some auto clear over the whole part?
possible Towel
possible Towel
Junior Member (17 reputation)Junior Member (17 reputation)Junior Member (17 reputation)Junior Member (17 reputation)Junior Member (17 reputation)Junior Member (17 reputation)Junior Member (17 reputation)Junior Member (17 reputation)Junior Member (17 reputation)
Group: Forum Members
Posts: 3, Visits: 44
thanks for the help!
Matthieu Libeert
Matthieu Libeert
Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
you can just sand it smooth and make a straight or chamfered finish Smile just use some sanding paper if you don't want to see the layers (if perhaps you used a core or Aramid or something) you can just 'paint' the edge with some coloured epoxy

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




possible Towel
possible Towel
Junior Member (17 reputation)Junior Member (17 reputation)Junior Member (17 reputation)Junior Member (17 reputation)Junior Member (17 reputation)Junior Member (17 reputation)Junior Member (17 reputation)Junior Member (17 reputation)Junior Member (17 reputation)
Group: Forum Members
Posts: 3, Visits: 44
I was just wondering, when finishing off large carbon pieces how do you make the edges (where cutting or drilling is required) look as good as the rest of the piece. As in, during the video tutorial for the carbon bonnet they cut and trimmed the edges but this would leave quite a large amount of scuffing, no?