I was just wondering, when finishing off large carbon pieces how do you make the edges (where cutting or drilling is required) look as good as the rest of the piece. As in, during the video tutorial for the carbon bonnet they cut and trimmed the edges but this would leave quite a large amount of scuffing, no?