Group: Administrators
Posts: 2.5K,
Visits: 8.5K
|
Looking great as always!
You wont have any problems with the oil itself as long as its got a good sealing layer of epoxy inside. However, as oils age you often get combustion products contaminating the oils and they can slowly eat into epoxies. Vinylester resins seem to have a better chemical resistance than epoxies so you might want to coat the inside of your can with that to give you extra protection.
I cant imagine it being a major problem in the short term though as a catch can shouldnt be getting much oil through it anyway on a properly tuned engine with well managed crank case breather/ventilation system.
Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant
|