Hi I'm making a carbon sunroof bung which will be in two parts that I bond together at the end like the carbon bonnet video.
The top outward facing side will be carbon but I want to make the underside out of just fibreglass to cut costs 
My question is what resins do i use for just a fibreglass part?

Gel coat -Can I use any black gel coat?

Resin-Which resin is best for this?

Fibreglass-do I have to use the powderd csm?

This is for wet layup 

Thanks for any help
Reply
Jdmleesy
Jdmleesy
Supreme Being (279 reputation)Supreme Being (279 reputation)Supreme Being (279 reputation)Supreme Being (279 reputation)Supreme Being (279 reputation)Supreme Being (279 reputation)Supreme Being (279 reputation)Supreme Being (279 reputation)Supreme Being (279 reputation)
Group: Forum Members
Posts: 39, Visits: 380
Well the carbon side I'm infusing iv already got all the stuff for that but I'm just on about the back panel for it where all the mounting points are.
 so if I get some black gelcoat, powderd csm and some epoxy resin and wet lay the back will that be good enough u think?