By Jdmleesy - 2/1/2014 11:11:31 AM

Hi I'm making a carbon sunroof bung which will be in two parts that I bond together at the end like the carbon bonnet video.
The top outward facing side will be carbon but I want to make the underside out of just fibreglass to cut costs 
My question is what resins do i use for just a fibreglass part?

Gel coat -Can I use any black gel coat?

Resin-Which resin is best for this?

Fibreglass-do I have to use the powderd csm?

This is for wet layup 

Thanks for any help
By Jdmleesy - 2/1/2014 1:58:12 PM

Or do u mean use polyester resin and woven glass because I do have 300g woven glass