How many layers? Jet ski


Author
Message
Mbalducci1990
Mbalducci1990
Forum Member (35 reputation)Forum Member (35 reputation)Forum Member (35 reputation)Forum Member (35 reputation)Forum Member (35 reputation)Forum Member (35 reputation)Forum Member (35 reputation)Forum Member (35 reputation)Forum Member (35 reputation)
Group: Forum Members
Posts: 5, Visits: 46
I have whats called a Waterdawg Kustomz hull, it is a stand up jet ski. It is made of carbon fiber with a fiberglass core. I have a bit of a project going on right now. The rear of the sky has a "sealed" cavity filled with foam that got somewhat waterlogged. I cut open the ski, removed all the foam, sealed it and foamed it. Now I am reinstalling the tray but im unsure how many layers of carbon fiber to use. I ordered some 19.7oz 2x2 twill from US Composites. I cut out 2 pieces for the bottom and for the gunwhales I am thinking 2 pieces as well. How would you go about doing this? Here's some pictures so it's easy to understand. The last photo isnt laid down yet, it's just 2 layers I cut out.












Reply
ajb100
ajb100
Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)
Group: Forum Members
Posts: 346, Visits: 4.4K
Welcome to the forum!

As the new carbon is just holding down the original floor, two layers will be fine