Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
General Composites Discussion
»
How many layers? Jet ski
How many layers? Jet ski
Post Reply
Like
3
How many layers? Jet ski
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
Mbalducci1990
Mbalducci1990
posted 11 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 5,
Visits: 46
I have whats called a Waterdawg Kustomz hull, it is a stand up jet ski. It is made of carbon fiber with a fiberglass core. I have a bit of a project going on right now. The rear of the sky has a "sealed" cavity filled with foam that got somewhat waterlogged. I cut open the ski, removed all the foam, sealed it and foamed it. Now I am reinstalling the tray but im unsure how many layers of carbon fiber to use. I ordered some 19.7oz 2x2 twill from US Composites. I cut out 2 pieces for the bottom and for the gunwhales I am thinking 2 pieces as well. How would you go about doing this? Here's some pictures so it's easy to understand. The last photo isnt laid down yet, it's just 2 layers I cut out.
Reply
Like
3
Reply
ajb100
ajb100
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 346,
Visits: 4.4K
Welcome to the forum!
As the new carbon is just holding down the original floor, two layers will be fine
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
How many layers? Jet ski
Mbalducci1990
-
11 Years Ago
Welcome to the forum! As the new carbon is just holding down the original floor, two layers will...
ajb100
-
11 Years Ago
Thanks. Good to hear 2 layers will be plenty. The enclosures on the sides are called "footholds" and...
Mbalducci1990
-
11 Years Ago
Well yesterday I put the jet ski in my boiler room at 75F and got it all laid up. Today, a little...
Mbalducci1990
-
11 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search