Hi there, thought I would join up see what projects like minded people have.

I'm a pre-preg laminator working within the Motorsport industry focusing mainly on automotive and F1
Before this I was working in the aerospace industry I've been laminating 2 years

Pictures are limited but I have a couple I can upload 

Fresh out the mould mainly 

Mclaren mp4 rear wing straight from break out 

Nissan GTR rear bumper again straight from the mould 

And a random fuel flap I made for my Golf

Instagram - C14ENN
Edited 11 Years Ago by Chenn
Chenn
Chenn
Forum Guru (54 reputation)Forum Guru (54 reputation)Forum Guru (54 reputation)Forum Guru (54 reputation)Forum Guru (54 reputation)Forum Guru (54 reputation)Forum Guru (54 reputation)Forum Guru (54 reputation)Forum Guru (54 reputation)
Group: Forum Members
Posts: 10, Visits: 191


A bit of texalium 
 

Sorry they aren't the most interesting photos but I'm not allowed to photograph the really good stuff. 

Here's a part ready for the auto clave for a certain new hybrid super car..



Cheers

Instagram - C14ENN
Chenn
Chenn
Forum Guru (54 reputation)Forum Guru (54 reputation)Forum Guru (54 reputation)Forum Guru (54 reputation)Forum Guru (54 reputation)Forum Guru (54 reputation)Forum Guru (54 reputation)Forum Guru (54 reputation)Forum Guru (54 reputation)
Group: Forum Members
Posts: 10, Visits: 191
Few bits from the aerospace days 

A full carbon satellite next to my previous mk2 golf






And a Mazda badge I did for a friend 



Instagram - C14ENN
Matthieu Libeert
Matthieu Libeert
Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
Thats some pretty amazing stuff you made! How do you cure such big parts?
to bad the satelite is painted BigGrin

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




Chenn
Chenn
Forum Guru (54 reputation)Forum Guru (54 reputation)Forum Guru (54 reputation)Forum Guru (54 reputation)Forum Guru (54 reputation)Forum Guru (54 reputation)Forum Guru (54 reputation)Forum Guru (54 reputation)Forum Guru (54 reputation)
Group: Forum Members
Posts: 10, Visits: 191
Thank you! 

All vacuum bagged and cured in a clave, we have 5 claves of varying sizes so room isn't an problem Smile 

Instagram - C14ENN
ajb100
ajb100
Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)
Group: Forum Members
Posts: 346, Visits: 4.4K
Recognise that bumper from edition 38 Wink
Chenn
Chenn
Forum Guru (54 reputation)Forum Guru (54 reputation)Forum Guru (54 reputation)Forum Guru (54 reputation)Forum Guru (54 reputation)Forum Guru (54 reputation)Forum Guru (54 reputation)Forum Guru (54 reputation)Forum Guru (54 reputation)
Group: Forum Members
Posts: 10, Visits: 191
Good old edition! Shows how little pictures I have at the moment but I have an interview for a new company tomorrow hoping that goes well! 

Instagram - C14ENN
NikCFC
NikCFC
Supreme Being (483 reputation)Supreme Being (483 reputation)Supreme Being (483 reputation)Supreme Being (483 reputation)Supreme Being (483 reputation)Supreme Being (483 reputation)Supreme Being (483 reputation)Supreme Being (483 reputation)Supreme Being (483 reputation)
Group: Forum Members
Posts: 61, Visits: 871
Wow! amazing parts for amazing machines!!! keep us posted!!!
Edited 11 Years Ago by NikCFC
fgayford
fgayford
Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)
Group: Forum Members
Posts: 433, Visits: 1.2K
Chenn (08/01/2014)
Thank you! 

All vacuum bagged and cured in a clave, we have 5 claves of varying sizes so room isn't an problem Smile 


Hello

Thanks for posting pictures, please keep them coming! Very very nice work!

Would you mind answering a few questions?

1  In your autoclave what PSI pressure do you use?

2  What temperature schedule do you use and max temp?

3  Do you do the surface layer in one shot and then build up the bulk of your thickness in a second shot?

4 Or do you do it all in one shot?

5 Do you allow a debulking time under full vacuum before you put it in the autoclave?

Thanks a million!

Fred 

GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search