Talk Composites - The Forum for Advanced Composites
Home
»
Advanced Composites Forum
»
New Member Introductions
New from England with pictures
http://www.talkcomposites.com/Topic9105.aspx
By Chenn
-
1/8/2014 2:43:42 PM
Hi there, thought I would join up see what projects like minded people have.
I'm a pre-preg laminator working within the Motorsport industry focusing mainly on automotive and F1
Before this I was working in the aerospace industry I've been laminating 2 years
Pictures are limited but I have a couple I can upload
Fresh out the mould mainly
Mclaren mp4 rear wing straight from break out
Nissan GTR rear bumper again straight from the mould
And a random fuel flap I made for my Golf
By fgayford
-
1/12/2014 7:53:39 PM
Chenn (08/01/2014)
Thank you!
All vacuum bagged and cured in a clave, we have 5 claves of varying sizes so room isn't an problem
Hello
Thanks for posting pictures, please keep them coming! Very very nice work!
Would you mind answering a few questions?
1 In your autoclave what PSI pressure do you use?
2 What temperature schedule do you use and max temp?
3 Do you do the surface layer in one shot and then build up the bulk of your thickness in a second shot?
4 Or do you do it all in one shot?
5 Do you allow a debulking time under full vacuum before you put it in the autoclave?
Thanks a million!
Fred