Mould Making
»
Making a mould from Campervan Headliner
Making a mould from Campervan Headliner
Post Reply
Like
9
Making a mould from Campervan Headliner
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
Skytiger
Skytiger
posted 14 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 7,
Visits: 51
Here is a picture of my headliner in my Baywindow campervan. Ignore the grining idiot thats me
So my thinking is to remove from campervan, it's going to be quite flexible when I remove it so some sort of frame would need to be made for it to hold it rigid. It is material surface so I need to cover it in something so the mold doesn't stick to it. Suggestions on materials to use for this and also what to use to make the mold.
I realise that what I put on it won't give me a perfect surface but I would need to take a part from the mould early on and modify it(materials to use for modifictions?ie.Foam/GRP) as I want to put speakers in it, nothing huge just 10cm speakers as I don't like them in the doors. Also to remove the indents for the handles, I don't use them anyway. I have a pop top fited aswell this has a wooden frame that goes around the roof you can see it in the top right corner of my picture I would like to blend it into the headliner for better asthetics. Once I had done that and got it shiny and glossy then make another mould from my modified headliner.
This would be the mould to take my final modified headliner part from.
Is this the right way to go about it,? Did any of this make sense? It is attached through holes with plastic bungs originally ideas on hidden fixings for these as the front is held on with the sunvisors which are screwed.
Edited
14 Years Ago by
Skytiger
Reply
Like
9
Reply
Joe
Joe
posted 14 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 310,
Visits: 1.5K
Hi,
I would first add all the shapes I want using foam glued to the the headliner and then sanded to shape.
Then, I would try to build a wooden structure glued to good side to try to rigidify it. Then remove the headliner, then build a stronger structure on the backside to allow removing the first structure without losing the shape.
Then its a matter of smoothing the good side. A first try with sanding paper to check if the fluffies can go ? Then a filler (2k, not from a spray can) then smooth.
I had hard times to remember where I did see that, but here's a link that might give you some ideas, but that would be more a "build from scratch" point of view.
I dont like those bling bling guys, but hey, tips might even be where you dont think they are
http://www.youtube.com/watch?v=CZzydukst_w&feature=related
 
 
    A $1000 electronic device will always protect a 10 cents fuse
Reply
Like
8
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Making a mould from Campervan Headliner
Skytiger
-
14 Years Ago
Hi, Iwould first add all the shapes I want using foam glued to the the headliner and then sanded...
Joe
-
14 Years Ago
Hi Skytiger, You've got the plan right and I'm basically with Joe on the method. It depends how...
Matt (Staff)
-
14 Years Ago
Thanks Joe and Matt, [quote][b]Matt (Staff) (01/03/2012)[/b][hr]Making a mould of the pattern (the...
Skytiger
-
14 Years Ago
Post Reply
Like
9
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search