Here is a picture of my headliner in my Baywindow campervan. Ignore the grining idiot thats meWink

http://www.talkcomposites.com/Uploads/Images/2b1405ee-605a-4e53-b839-2f36.jpg

So my thinking is to remove from campervan, it's going to be quite flexible when I remove it so some sort of frame would need to be made for it to hold it rigid.  It is material surface so I need to cover it in something so the mold doesn't stick to it.  Suggestions on materials to use for this and also what to use to make the mold.

I realise that what I put on it won't give me a perfect surface but I would need to take a part from the mould early on and modify it(materials to use for modifictions?ie.Foam/GRP) as I want to put speakers in it, nothing huge just 10cm speakers as I don't like them in the doors.  Also to remove the indents for the handles, I don't use them anyway.  I have a pop top fited aswell this has a wooden frame that goes around the roof you can see it in the top right corner of my picture I would like to blend it into the headliner for better asthetics. Once I had done that and got it shiny and glossy then make another mould from my modified headliner.

This would be the mould to take my final modified headliner part from.

Is this the right way to go about it,? Did any of this make sense? It is attached through holes with plastic bungs originally ideas on hidden fixings for these as the front is held on with the sunvisors which are screwed.
Edited 13 Years Ago by Skytiger
Reply
Joe
Joe
Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)
Group: Forum Members
Posts: 310, Visits: 1.5K
Hi,

I would first add all the shapes I want using foam glued to the the headliner and then sanded to shape.

Then, I would try to build a wooden structure glued to good side to try to rigidify it. Then remove the headliner, then build a stronger structure on the backside to allow removing the first structure without losing the shape.

Then its a matter of smoothing the good side. A first try with sanding paper to check if the fluffies can go ? Then a filler (2k, not from a spray can) then smooth.

I had hard times to remember where I did see that, but here's a link that might give you some ideas, but that would be more a "build from scratch" point of view.

I dont like those bling bling guys, but hey, tips might even be where you dont think they are Wink

http://www.youtube.com/watch?v=CZzydukst_w&feature=related

 



 


    A $1000 electronic device will always protect a 10 cents fuse
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search