hi! 

I had a problem trying to cover with carbon the tailgate of my citroen C4

Before applying the black gelcoat, sand it and clean it thoroughly, then apply and let dry carbon, after 3 days drying, I began to smooth the carbon layer, but note that in an area came as a bubble, but it was the carbon that had taken off from the part

Now already removed all carbon, and sanded again, but the layer appeared after removing the carbon is not the same as that in the first sand

As I can do to cover this piece? had planned to do with polyester?

See if you can help




Thanks
Reply
loy
loy
Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)
Group: Awaiting Activation
Posts: 4, Visits: 447
hi thanks for your answers 

I think the problem that is to come up paint that came in the trunk, the basecoat lifted well in the part, typically carbon already pressed against the basecoat. Now the piece is clean, there is only one layer of a kind of black paint primer will, and in some places only the plastic

I'll upload photos later

What should I do now? abrade with 80 back to start?