problems with skinning


Author
Message
loy
loy
Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)
Group: Awaiting Activation
Posts: 4, Visits: 447
hi! 

I had a problem trying to cover with carbon the tailgate of my citroen C4

Before applying the black gelcoat, sand it and clean it thoroughly, then apply and let dry carbon, after 3 days drying, I began to smooth the carbon layer, but note that in an area came as a bubble, but it was the carbon that had taken off from the part

Now already removed all carbon, and sanded again, but the layer appeared after removing the carbon is not the same as that in the first sand

As I can do to cover this piece? had planned to do with polyester?

See if you can help




Thanks
Reply
TomDesign
TomDesign
Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)
Group: Forum Members
Posts: 454, Visits: 2.5K
i think it was paint that started to come out on a part and that cause these things reaction. so always sand those things and try to brush paper dry like 80-100 grid