I need to mod a plenum, It is from a Formula A1 race engine, I need to add some reinforcements to it, what is the best way to go.
Either build up with pre preg or to do a hand layup, if pre preg what would be the best way to bond it, I can oven cure un bagged.

Alan
Reply
Shaneer22
Shaneer22
Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)
Group: Forum Members
Posts: 156, Visits: 14K
As far as iam aware Same principle key are 80 120 clean surface acetone,ready to bond. 