Bonding to Cured Pre Preg

http://www.talkcomposites.com/Topic9024.aspx

By Alan Whitaker - 1/3/2014 5:41:40 AM

I need to mod a plenum, It is from a Formula A1 race engine, I need to add some reinforcements to it, what is the best way to go.
Either build up with pre preg or to do a hand layup, if pre preg what would be the best way to bond it, I can oven cure un bagged.

Alan
By Shaneer22 - 1/3/2014 11:23:27 AM

As far as iam aware Same principle key are 80 120 clean surface acetone,ready to bond.