Looks like a fun project!
One thing i will say is plan your mould flanges and mould split lines very carefully to ensure no mechanical lock and also easy demoulding and mould assembly. You have to make your moulds such that you can assemble it and it holds the shape accurately. You can use wooden battens on the reverse to further stiffen the moulds up.
Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant
|