A few months back I made some cycle wings with red gelcoat edges for a customer with a Westfield sportscar. I have just completed a dashboard using the same technique. They are done using pigmented GC50 sprayed into the mould before infusion. It has taken some experimentation to get the timing right. Remove the masking tape too soon and you loose the crisp edge of the line, leave it too long and the gelcoat will lift from the mould when you remove the masking tape.

Warren

Carbon Copies Ltd
Replies
dbcrx
dbcrx
Supreme Being (362 reputation)Supreme Being (362 reputation)Supreme Being (362 reputation)Supreme Being (362 reputation)Supreme Being (362 reputation)Supreme Being (362 reputation)Supreme Being (362 reputation)Supreme Being (362 reputation)Supreme Being (362 reputation)
Group: Forum Members
Posts: 46, Visits: 1.2K
nice. did you spray clear gel over the rest of the mould as well or just the red?
wozza
wozza
Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)
Group: Forum Members
Posts: 688, Visits: 5.4K
dbcrx (12/12/2013)
nice. did you spray clear gel over the rest of the mould as well or just the red?



Hi, on the cycle wings the red went down first followed by clear GC50 to help with stone chips/UV. On the dash I just did a resin rich infusion after the red had tacked off.

Warren

Carbon Copies Ltd
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search