Cutting cured carbon?


Author
Message
StanTheMan
StanTheMan
Supreme Being (455 reputation)Supreme Being (455 reputation)Supreme Being (455 reputation)Supreme Being (455 reputation)Supreme Being (455 reputation)Supreme Being (455 reputation)Supreme Being (455 reputation)Supreme Being (455 reputation)Supreme Being (455 reputation)
Group: Forum Members
Posts: 61, Visits: 380
I'm using Dremel 3000 along with a diamond wheel which is not cheap either at around 20EUR. It does the trick for about 30-40cm and then goes dull. It only cuts when the dremel is at it's highest setting. Anything less and it barely scratches the surface. It seems as if when the resin is heated while cutting, it sticks on the wheel and dulls it. I don't know if that's whats happening but I can see that the dimond wheel is covered with thick black stuff. I can sand it down with some abrasive paper but that doesn't seem to improve anything. Can anybody help me with that? Any methods for cleaning/sharpening the diamond wheel? 
Replies
Brian_s
Brian_s
Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)
Group: Forum Members
Posts: 99, Visits: 2.5K
Expensive? Try these.

http://www.ebay.co.uk/itm/TZ-6PC-MINI-Diamond-Cutting-Discs-Fit-Rotary-Tool-Mini-Dremel-Drills-Cut-Off-/190612661602?pt=UK_Home_Garden_PowerTools_SM&hash=item2c61666562

I tried the Perma-grit disks but found them too coarse.

Also, if residue is sticking to the disks is your work cured fully?

Brian.
wojtepanik
wojtepanik
Supreme Being (755 reputation)Supreme Being (755 reputation)Supreme Being (755 reputation)Supreme Being (755 reputation)Supreme Being (755 reputation)Supreme Being (755 reputation)Supreme Being (755 reputation)Supreme Being (755 reputation)Supreme Being (755 reputation)
Group: Forum Members
Posts: 102, Visits: 582
Brian_s (09/12/2013)
Expensive? Try these.

http://www.ebay.co.uk/itm/TZ-6PC-MINI-Diamond-Cutting-Discs-Fit-Rotary-Tool-Mini-Dremel-Drills-Cut-Off-/190612661602?pt=UK_Home_Garden_PowerTools_SM&hash=item2c61666562

I tried the Perma-grit disks but found them too coarse.

Also, if residue is sticking to the disks is your work cured fully?

Brian.

Yeah maybe it is cheaper but I pay 0,25 euro for one and it never let me down. I would love to try perma-grit but they are out of my reach, because shipping to poland is too expensive, I am collecting order and I will order bigger parcel at once to save money ;D

~~~Everytime I hear sound of demoulding part I have eargasm~~~
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
StanTheMan - 12 Years Ago
wojtepanik - 12 Years Ago
Brian_s - 12 Years Ago
wojtepanik - 12 Years Ago
Warren (Staff) - 12 Years Ago
baja_patient - 12 Years Ago
dbcrx - 12 Years Ago
StanTheMan - 12 Years Ago
wojtepanik - 12 Years Ago
wojtepanik - 12 Years Ago
dbcrx - 12 Years Ago
macgtech - 11 Years Ago
fgayford - 11 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search