Hi! I don't really use diamond wheel because it is too expensive and too fragile to work. I use the simpliest cutting wheels and they work really well, but they get too small to use quiet fast. Another thing is that your dremel has not enough power to cut through thin laminate. Invest in more powerfull dremel and disposable cutting wheels. Bye Wojtek from Poland