Hi, pre preg is not thermo plastic. You should store fabric in fridge just to increase amount of storage time. Pre preg is a cf fabric pre saturated with mixed epoxy, with veryyy slow hardener. You heat the pre preg to cure it faster ( it would cure in room temp. but I quess it would take couple weeks) in oven it takes about 8h to fully cure. You can roll it just as a normal fabric, Bye Wojtek from Poland