I have attempted to cast a model using Easy Composites' Fast Cast Polyurethane Casting Resin. The cast failed as the resin did not fully cure. Half the model cured but the rest came out like thick honey, see image above. I'm not sure why this happened, but my immediate problem is, how do I clean the uncured resin goo from my mold? The mold is made of RTV silicone.

Edited 13 Years Ago by moif
Reply
Matthieu Libeert
Matthieu Libeert
Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
How long did you cure and at which temperature? 
It can be quit a mess to clean :s I would try to clean it with acetone...
If you think you mixed the A+B well at good ratios you could still try to put it into an oven or hope for it to fully cure

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search