Problems with carbon skinning


Author
Message
wojtepanik
wojtepanik
Supreme Being (755 reputation)Supreme Being (755 reputation)Supreme Being (755 reputation)Supreme Being (755 reputation)Supreme Being (755 reputation)Supreme Being (755 reputation)Supreme Being (755 reputation)Supreme Being (755 reputation)Supreme Being (755 reputation)
Group: Forum Members
Posts: 102, Visits: 582
Sure, no problem
Bye 
Wojtek from Poland

~~~Everytime I hear sound of demoulding part I have eargasm~~~
TomDesign
TomDesign
Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)
Group: Forum Members
Posts: 454, Visits: 2.5K
nothing helping me i treyed lot of resins and gelcoats 5 years and can not get what other use for perfect hard part finish . as anyway pin holes appear.
TomDesign
TomDesign
Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)
Group: Forum Members
Posts: 454, Visits: 2.5K








Look how bad surface comparing to one company that wrap. if we use epoxy at +20 all the time same 4 times same. polyster resin also bad. infusion resin also bad.

R-wraps
R-wraps
Forum Guru (60 reputation)Forum Guru (60 reputation)Forum Guru (60 reputation)Forum Guru (60 reputation)Forum Guru (60 reputation)Forum Guru (60 reputation)Forum Guru (60 reputation)Forum Guru (60 reputation)Forum Guru (60 reputation)
Group: Forum Members
Posts: 10, Visits: 172
Mine is similar but polished up reasonably well
R-wraps
R-wraps
Forum Guru (60 reputation)Forum Guru (60 reputation)Forum Guru (60 reputation)Forum Guru (60 reputation)Forum Guru (60 reputation)Forum Guru (60 reputation)Forum Guru (60 reputation)Forum Guru (60 reputation)Forum Guru (60 reputation)
Group: Forum Members
Posts: 10, Visits: 172
Here's a pic
Attachments
image.jpg (196 views, 641.00 KB)
TomDesign
TomDesign
Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)
Group: Forum Members
Posts: 454, Visits: 2.5K
yes but we here not to do bad finish but exchange some ideas and to run perfect stuff
R-wraps
R-wraps
Forum Guru (60 reputation)Forum Guru (60 reputation)Forum Guru (60 reputation)Forum Guru (60 reputation)Forum Guru (60 reputation)Forum Guru (60 reputation)Forum Guru (60 reputation)Forum Guru (60 reputation)Forum Guru (60 reputation)
Group: Forum Members
Posts: 10, Visits: 172
Here's my second attempt used a clear coat too finish
Attachments
image.jpg (171 views, 981.00 KB)