R-wraps
R-wraps
posted 12 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 10,
Visits: 172
Just started my first go at carbon skinning and it appears that it's going to need a lot of resin too smooth it out as after 2 Coates the carbon is still sticking through the resin
Reply
Like
3
benet
benet
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 59,
Visits: 373
what grade is the carbon ?
Reply
Like
2
R-wraps
R-wraps
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 10,
Visits: 172
2 x 2 twil 3k it's the stuff you get in the carbon mods skinning kits
Reply
Like
3
benet
benet
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 59,
Visits: 373
dont know then.. i had a similar problem with 450gsm but thats because it was so heavy.
Reply
Like
3
wojtepanik
wojtepanik
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 102,
Visits: 582
benet (10/11/2013)
dont know then.. i had a similar problem with 450gsm but thats because it was so heavy.
dude, how you can wrap something with 450gsm? o.O
~~~Everytime I hear sound of demoulding part I have eargasm~~~
Reply
Like
2
R-wraps
R-wraps
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 10,
Visits: 172
Does carbon fiber swell with resin
Reply
Like
3
wojtepanik
wojtepanik
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 102,
Visits: 582
R-wraps (10/11/2013)
Does carbon fiber swell with resin
resin gets between single strands of cf, so it is hard to anwser, I would say no but as I said resin gets between strands :o
~~~Everytime I hear sound of demoulding part I have eargasm~~~
Reply
Like
3
R-wraps
R-wraps
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 10,
Visits: 172
That makes more sense so approx 4 costs of resin. What's the best way to avoid pin pricks?
Reply
Like
3
wojtepanik
wojtepanik
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 102,
Visits: 582
to avoid pin holes you have to use less sticky resin or heat up your resin or use tiny brush to fill all the pinholes with resin
~~~Everytime I hear sound of demoulding part I have eargasm~~~
Reply
Like
2
R-wraps
R-wraps
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 10,
Visits: 172
That's awesome that bud thanks very much for your help
Reply
Like
2
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
3
1
2
Next
Jump To Page
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search