Just started my first go at carbon skinning and it appears that it's going to need a lot of resin too smooth it out as after 2 Coates the carbon is still sticking through the resin
Reply
R-wraps
R-wraps
Forum Guru (60 reputation)Forum Guru (60 reputation)Forum Guru (60 reputation)Forum Guru (60 reputation)Forum Guru (60 reputation)Forum Guru (60 reputation)Forum Guru (60 reputation)Forum Guru (60 reputation)Forum Guru (60 reputation)
Group: Forum Members
Posts: 10, Visits: 172
Here's my second attempt used a clear coat too finish
Attachments
image.jpg (170 views, 981.00 KB)
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
R-wraps - 12 Years Ago
benet - 12 Years Ago
R-wraps - 12 Years Ago
benet - 12 Years Ago
wojtepanik - 12 Years Ago
R-wraps - 12 Years Ago
wojtepanik - 12 Years Ago
R-wraps - 12 Years Ago
wojtepanik - 12 Years Ago
R-wraps - 12 Years Ago
             Sure, no problem Bye Wojtek from Poland
wojtepanik - 12 Years Ago
TomDesign - 12 Years Ago
     ...
TomDesign - 12 Years Ago
R-wraps - 12 Years Ago
     Here's a pic
R-wraps - 12 Years Ago
TomDesign - 12 Years Ago
R-wraps - 12 Years Ago