By R-wraps - 11/9/2013 9:11:40 PM
Just started my first go at carbon skinning and it appears that it's going to need a lot of resin too smooth it out as after 2 Coates the carbon is still sticking through the resin
|
By R-wraps - 11/17/2013 8:19:12 PM
Here's my second attempt used a clear coat too finish
|
|