Hi
last week I was making a mould but on had to go away very unexpectedly without finishing the mould,  tooling gelcoat had gone in wednesday + has been left till now, can it over cure rendering it useless or will I be ok laying up coupling coat + reinforcement as usual?
Thanks
Reply
James66
James66
Supreme Being (82 reputation)Supreme Being (82 reputation)Supreme Being (82 reputation)Supreme Being (82 reputation)Supreme Being (82 reputation)Supreme Being (82 reputation)Supreme Being (82 reputation)Supreme Being (82 reputation)Supreme Being (82 reputation)
Group: Forum Members
Posts: 10, Visits: 99
Hi guys
Sorry I didnt update

mod came out absolutely fine, thanks for the help + advice, it may well have saved it

james
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search