can gelcoat over cure?


Author
Message
James66
James66
Supreme Being (82 reputation)Supreme Being (82 reputation)Supreme Being (82 reputation)Supreme Being (82 reputation)Supreme Being (82 reputation)Supreme Being (82 reputation)Supreme Being (82 reputation)Supreme Being (82 reputation)Supreme Being (82 reputation)
Group: Forum Members
Posts: 10, Visits: 99
Hi guys
Sorry I didnt update

mod came out absolutely fine, thanks for the help + advice, it may well have saved it

james
carboncactus
carboncactus
Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)
Group: Forum Members
Posts: 243, Visits: 1K
Addint ot what Warren said, if its not tacky at all, give it a very light wipe with some acetone, it will be slightly tacky again for a briem period, enough to lay another coat on.

http://www.talkcomposites.com/Uploads/Images/db628ad5-e0e7-47b9-873a-3d84.png
Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
You are best doing it within a reasonable time, usually within a day. This ensures there is proper cross linking.  You can rough up the surface of the gel and work from there and hopefully you will be ok.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
James66
James66
Supreme Being (82 reputation)Supreme Being (82 reputation)Supreme Being (82 reputation)Supreme Being (82 reputation)Supreme Being (82 reputation)Supreme Being (82 reputation)Supreme Being (82 reputation)Supreme Being (82 reputation)Supreme Being (82 reputation)
Group: Forum Members
Posts: 10, Visits: 99
Hi
last week I was making a mould but on had to go away very unexpectedly without finishing the mould,  tooling gelcoat had gone in wednesday + has been left till now, can it over cure rendering it useless or will I be ok laying up coupling coat + reinforcement as usual?
Thanks
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search