By James66 - 9/16/2013 8:43:17 AM

Hi
last week I was making a mould but on had to go away very unexpectedly without finishing the mould,  tooling gelcoat had gone in wednesday + has been left till now, can it over cure rendering it useless or will I be ok laying up coupling coat + reinforcement as usual?
Thanks
By James66 - 10/16/2013 8:26:06 PM

Hi guys
Sorry I didnt update

mod came out absolutely fine, thanks for the help + advice, it may well have saved it

james