Brushed on GC50


Author
Message
Brian_s
Brian_s
Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)
Group: Forum Members
Posts: 99, Visits: 2.5K
Hi, I have just painted my mould in GC50. I got it as smooth as I could with an Easy Composites disposable brush. Now it has set it looks like a ploughed field. I assume that these ridges will distort the carbon fabric and show in the finished product.
Should I try rubbing them down or fill them with GC50 thinned with acetone?
Any other suggestions would be appreciated.

Brian.
Edited 12 Years Ago by Brian_s
Reply
Brian_s
Brian_s
Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)
Group: Forum Members
Posts: 99, Visits: 2.5K
It must be the light. This is a picture of the other side. The patches are clouds.

Brian.

http://www.talkcomposites.com/Uploads/Images/e0a81a21-8d82-4759-888c-95d7.JPG
Edited 12 Years Ago by Brian_s