Brian_s
Brian_s
posted 12 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 99,
Visits: 2.5K
Hi, I have just painted my mould in GC50. I got it as smooth as I could with an Easy Composites disposable brush. Now it has set it looks like a ploughed field. I assume that these ridges will distort the carbon fabric and show in the finished product.
Should I try rubbing them down or fill them with GC50 thinned with acetone?
Any other suggestions would be appreciated.
Brian.
Edited
12 Years Ago by
Brian_s
Reply
Like
3
Reply
Warren (Staff)
Warren (Staff)
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Administrators
Posts: 2.5K,
Visits: 8.5K
Doesnt look too bad. Is it dull and needing a polish or is that just the light??
Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Reply
Like
2
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Brushed on GC50
Brian_s
-
12 Years Ago
OK, Answering my own post. I rubbed it down as much as I dared as I didn't want to go through the...
Brian_s
-
12 Years Ago
Hi Brian S The best way to apply G50 is by spray, if you look on the gel coat tub is says do NOT re...
carbonfibreworks
-
12 Years Ago
Can you post spray, or does it have to be in mold before layup?
cpkielycua
-
12 Years Ago
We always recommend spraying GC50 for infusion. Spray it into the mould at the same stage you brush...
Warren (Staff)
-
12 Years Ago
This can only be sprayed properly. But make sure you take all the necessary safety precautions....
baja_patient
-
12 Years Ago
Thank you for the advice. I can't afford a Gelcoat spray gun at the moment. It looks like I have...
Brian_s
-
12 Years Ago
Doesnt look too bad. Is it dull and needing a polish or is that just the light??
Warren (Staff)
-
12 Years Ago
It must be the light. This is a picture of the other side. The patches are clouds. Brian.
Brian_s
-
12 Years Ago
I have bonded the 2 halves of this together with PT326. I have cleaned up the seam but would like to...
Brian_s
-
12 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search