Group: Forum Members
Posts: 99,
Visits: 2.5K
|
Hi, I have just painted my mould in GC50. I got it as smooth as I could with an Easy Composites disposable brush. Now it has set it looks like a ploughed field. I assume that these ridges will distort the carbon fabric and show in the finished product. Should I try rubbing them down or fill them with GC50 thinned with acetone? Any other suggestions would be appreciated.
Brian.
|