Hi there,
I am pretty new to working with carbon, but have a good background in other materials.

I am working on designing a strutted framework, fabricated out of 5mm pultruded carbon tube, and I thought it best to seek some advice about how best to make the joints. My plan is to build a jig which holds everything flat, and use a braided sleeve to form a reinforced skin. However since I also plan on painting the structure, I don't necessarily need the braid for aesthetics, however I also don't want 'spider knees' at each join. 

To simplify things, lets assume i am building a small chair, with some structural triangulation, which needs to hold about 10kg ( so in real world terms I guess it has to be over-engineered to not fail under 50kg, or something of the kind ).

In my crude drawing I have 3 potential jointing processes, but I wonder if there is another I have not considered, or if I would be better off making a mould and a core, and using a cast component joined by tubes, rather than attempting to join struts together. 

Thanks,
T
Attachments
image.jpg (891 views, 114.00 KB)
Replies
carbonfibreworks
carbonfibreworks
Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)
Group: Forum Members
Posts: 292, Visits: 4.5K
Hello Tobias
I have used the above adhesive on the top fairing mount on my classic racing motorcycle, i used it to join 10mm carbon tube to a piece of  pre preg plate . I abraded the parts to be bonded with 180 grit paper and the part is under load and the joint has been 100% reliable.
Regards Chris
carbonfibreworks.co.uk

http://www.talkcomposites.com/Uploads/Images/97e08777-693c-4af1-a27a-86cf.png
Tobias
Tobias
Forum Member (48 reputation)Forum Member (48 reputation)Forum Member (48 reputation)Forum Member (48 reputation)Forum Member (48 reputation)Forum Member (48 reputation)Forum Member (48 reputation)Forum Member (48 reputation)Forum Member (48 reputation)
Group: Forum Members
Posts: 6, Visits: 16
Hmm, this was a 20mm carbon tube, and the join was to a strut coming in below, by means of an aluminium sleeve which wrapped around the tube like a clamp - made from 20x2mm stock.
carbonfibreworks
carbonfibreworks
Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)
Group: Forum Members
Posts: 292, Visits: 4.5K
I will post an image of the part on Friday.
Regards Chris
carbonfibreworks.co.uk

http://www.talkcomposites.com/Uploads/Images/97e08777-693c-4af1-a27a-86cf.png
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
Tobias - 12 Years Ago
Warren (Staff) - 12 Years Ago
Tobias - 12 Years Ago
Warren (Staff) - 12 Years Ago
Tobias - 12 Years Ago
carbonfibreworks - 12 Years Ago
Tobias - 12 Years Ago
carbonfibreworks - 12 Years Ago
Shaneer22 - 12 Years Ago
Warren (Staff) - 12 Years Ago
ajb100 - 12 Years Ago
Tobias - 12 Years Ago
Warren (Staff) - 12 Years Ago
Tobias - 11 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search