Hi there,
I am pretty new to working with carbon, but have a good background in other materials.

I am working on designing a strutted framework, fabricated out of 5mm pultruded carbon tube, and I thought it best to seek some advice about how best to make the joints. My plan is to build a jig which holds everything flat, and use a braided sleeve to form a reinforced skin. However since I also plan on painting the structure, I don't necessarily need the braid for aesthetics, however I also don't want 'spider knees' at each join. 

To simplify things, lets assume i am building a small chair, with some structural triangulation, which needs to hold about 10kg ( so in real world terms I guess it has to be over-engineered to not fail under 50kg, or something of the kind ).

In my crude drawing I have 3 potential jointing processes, but I wonder if there is another I have not considered, or if I would be better off making a mould and a core, and using a cast component joined by tubes, rather than attempting to join struts together. 

Thanks,
T
Attachments
image.jpg (983 views, 114.00 KB)
Reply
Tobias
Tobias
Forum Member (48 reputation)Forum Member (48 reputation)Forum Member (48 reputation)Forum Member (48 reputation)Forum Member (48 reputation)Forum Member (48 reputation)Forum Member (48 reputation)Forum Member (48 reputation)Forum Member (48 reputation)
Group: Forum Members
Posts: 6, Visits: 16
Hi Warren,
So if you were to build such a structure, you would work with alloy inserts and a braided sleeve, or is there another approach that you would prefer? And should the inserts be glued in using the same epoxy resin as the wetting, or should they be made of a more flexible epoxy?

Cheers,
T
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
Tobias - 13 Years Ago
Warren (Staff) - 13 Years Ago
Tobias - 13 Years Ago
Warren (Staff) - 13 Years Ago
Tobias - 13 Years Ago
carbonfibreworks - 13 Years Ago
Tobias - 13 Years Ago
carbonfibreworks - 13 Years Ago
Shaneer22 - 13 Years Ago
Warren (Staff) - 13 Years Ago
ajb100 - 13 Years Ago
Tobias - 13 Years Ago
Warren (Staff) - 13 Years Ago
Tobias - 12 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search