Thermal Expansion Co-effecient: Pultruded vs Roll Wrapped


Author
Message
BenH
BenH
Forum Member (26 reputation)Forum Member (26 reputation)Forum Member (26 reputation)Forum Member (26 reputation)Forum Member (26 reputation)Forum Member (26 reputation)Forum Member (26 reputation)Forum Member (26 reputation)Forum Member (26 reputation)
Group: Forum Members
Posts: 2, Visits: 32
I'm looking to use a CF tube for a length critical application with absolute minimum axial thermal expansion, would pultruded or roll-wrapped be better for this application?
If there is any data regarding the thermal properties of each to compare the two types that'd be brilliant.
Reply
Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
There is no such data on the manufacturers information we have on our roll wrapped tubes.

To be frank, you will unlikely find that data freely available either as its a very specific application so the manufacturer is extremely unlikely to have bothered to measure those figures.

The Tubes do use a Toray T700 fibre so you may be able to find some data out there for the raw fibre and interpolate/calculate from there.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant