Thermal Expansion Co-effecient: Pultruded vs Roll Wrapped

http://www.talkcomposites.com/Topic7493.aspx

By BenH - 8/20/2013 12:18:31 PM

I'm looking to use a CF tube for a length critical application with absolute minimum axial thermal expansion, would pultruded or roll-wrapped be better for this application?
If there is any data regarding the thermal properties of each to compare the two types that'd be brilliant.
By compositepro - 8/21/2013 10:23:18 PM

its depends entirely what kind of accuracies you are looking at