Inflatable Bladder Mould


Author
Message
SergioLavalle01
SergioLavalle01
Forum Guru (61 reputation)Forum Guru (61 reputation)Forum Guru (61 reputation)Forum Guru (61 reputation)Forum Guru (61 reputation)Forum Guru (61 reputation)Forum Guru (61 reputation)Forum Guru (61 reputation)Forum Guru (61 reputation)
Group: Forum Members
Posts: 1, Visits: 5
Hi:

I want to make a hollow tube for an aerobar shaped lik " _/ "

I was thinking on making it with an inflatable blader and a epoxy mould sliced in 2.

What do you recomend?
Reply
H4RTM4N
H4RTM4N
Supreme Being (143 reputation)Supreme Being (143 reputation)Supreme Being (143 reputation)Supreme Being (143 reputation)Supreme Being (143 reputation)Supreme Being (143 reputation)Supreme Being (143 reputation)Supreme Being (143 reputation)Supreme Being (143 reputation)
Group: Forum Members
Posts: 7, Visits: 203
Hey guys,

This is a very interesting post. I want to make a long, hollow CF/EP tube to record with my GoPro. I could use an aluminum tube to make a half-mould. From there, I would make two halves and then glue them together. However, the joint would be visible and the tube wouldn't be as strong as a hollow, one-piece CF/EP tube. 

Using an Inflatable Bladder would certainly be the best idea. I carried out some research and I found some interesting videos/posts from a very clever guy that makes his own R/C planes.

Making an Inflation Bladder for Assisted Composite Part Fabrication

https://vimeo.com/10665397

Layup of The Wyoming Wind Works DLG Fuselage

https://vimeo.com/35648020

Demolding of the Wyoming Wind Works DLG Fuse

https://vimeo.com/37883424

I still don't understand how putting reinforcements and resin in each side of the mould separately ends up in a solid piece when the mould is closed. There has to be some overlapping that the bladder is pressing against the mould or another clever solution. Trying to find and answer to this, I found this interesting post:

Closed-Mold Vacuum Infusion with a Bladder

http://www.rcgroups.com/forums/showthread.php?t=1594856

Another way of doing this seems to be the following:
  1. Make the two-halves independently using joggle tools in each mould.
  2. Apply glue to the edges while the parts are still in the moulds.
  3. Close the moulds and apply pressure.
Check this post for more detailed information: http://www.rcgroups.com/forums/showpost.php?p=11804764&postcount=135

Has any of you guys made a one-piece hollow part using any of these techniques? I'm seeking for advice because I'm very new to this. 
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
SergioLavalle01 - 14 Years Ago
MAVERICK - 14 Years Ago
ant... - 14 Years Ago
matthieutje65 - 14 Years Ago
jim - 14 Years Ago
H4RTM4N - 13 Years Ago
mhdghoul - 14 Years Ago
Manu - 14 Years Ago
prsw - 14 Years Ago
Zebra - 10 Years Ago
ArturK - 8 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search